Stainless steel angle bar (V bar) – Decorative material for a modern – luxurious space.
With shiny properties, good anti-rust, especially easy to clean, and non-magnetic. Stainless steel V bar steel will definitely be a good choice for your interior space and construction space.
Learn more about stainless steel angle steel through this article on Tiger Steel!
Features and applications of stainless steel angle bar ( V bar)
Stainless steel angle with good corrosion resistance. High ductility, excellent tensile, forming, and spinning properties.
Especially non-magnetic, only becomes slightly magnetic when working at low temperatures.
The low carbon content means less carbide precipitation in the heat-affected zone. Especially during welding and the sensitivity to intergranular corrosion is lower.
In addition, the stainless steel angle bar is also resistant to most oxidizing acids and salt sprays. Things that can cause damage to your construction.

For angle steels made from 316 stainless steel, they are also resistant to sodium and calcium salt water. Resistant to hypochlorite solutions, phosphoric acid; sulfite alcohols, and sulfuric acids used in the pulp industry.
Thanks to such characteristics and strengths. Stainless steel angle steel is widely used in food and pharmaceutical processing rooms and marine exterior decorations.
In many luxury villas, a lot of stainless steel angle bar is also used to make interior and exterior decoration materials. Thanks to high aesthetics bring luxury to the house.
Types of steel used to make stainless steel angle bar
Stainless steel angle bar grade SUS201
Steel Type: Austenitic
Common name: Chromium-Manganese-Nickel Steel
Equivalent steel grades: ASME SA412, ASTM A276, ASTM A276, ASTM A412, ASTM A429, ASTM A666, FED QQ-S-766, SAE 30201, SAE J405 (30201), UNS S20100.
Chemical composition:
CHEMICAL COMPOSITION | |||
---|---|---|---|
Component | Weight% | ||
C | 0,15 | ||
Mn | 5,5-7,5 | ||
Si | 1 | ||
Cr | 16.0-18.0 | ||
Ni | 3,5-5,5 | ||
P | 0,06 | ||
S | 0,03 | ||
N | 0,25 | ||
Mechanical properties | |||
Characteristic | Conditions | ||
T (° C) | How to make | ||
Density (× 1000 kg / m 3 ) | 7.8 | 25 | |
Ratio Poisson | 0,27-0,30 | 25 | |
Elastic modulus (GPa) | 197 | 25 | |
Tensile (Mpa) | 515 | 25 | another annealing (plate, strip) |
Productive power (Mpa) | 275 | ||
Elongation (%) | 40 | ||
Reduce area (%) | 45 | ||
Thermal properties | |||
Characteristic | Conditions | ||
T (° C) | How to make | ||
Thermal expansion (10 -6 / ºC) | 15,7 | 0 – 100 half | |
Thermal conductivity (W / mK) | 16,2 | 100 nữa | |
Specific heat (J / kg-K) | 500 | 0 – 100 | |
Electrical properties | |||
Characteristic | Conditions | ||
T (° C) | How to make | ||
Resistivity (10 -9 W -m) | 690 | 25 |

Stainless steel angle bar grade SUS304
Equivalent steel grades: T304, SS304, 304SS, 304 SS, UNS S30400; AMS 5501/ 5513/ 5560/ 5565/ 5566/ 5567/ 5639/ 5697; ASME SA182/ SA194 (8)/ SA213/ SA240/ SA249/ SA312/ SA320 (B8)/ SA358/ SA376/ SA403/ SA409/ SA430/ SA479/ SA688; ASTM A167/ A182/ A193/ A194/ A666; FED QQ-S-763, MILSPEC MIL-S-5059, SAE 30304, DIN 1.4301, X5CrNi189, B.S. 304 S 15, EN 58E, PN 86020 (Poland), OH18N9, ISO 4954 X5CrNi189E, ISO 683/13 11, 18-8
Steel specifications:
Component | Concentration % |
C | Max 0.08 |
Cr | 18 – 20 |
Fe | 66.345 – 74 |
Mn | Max 2 |
Ni | 8 – 10.5 |
P | Max 0.045 |
S | Max 0.03 |
Si | Max 1 |
Physical properties | Metric system | pounds | Annotate |
Proportion | 8 g/cc | 0.289 lb/in³ | |
Mechanical properties | |||
Stiffness Brinell | 123 | 123 | Estimated value based on hardness Rockwell B |
StiffnessKnoop | 138 | 138 | Estimated value based on hardness Rockwell B. |
Stiffness Rockwell B | 70 | 70 | |
Stiffness Vickers | 129 | 129 | Estimated value based on hardness Rockwell B. |
tensile stress | 505 MPa | 73200 psi | |
Flow yield | 215 MPa | 31200 psi | at 0.2% offset |
Elongation | 70 % | 70 % | in 50 mm |
Modul đàn hồi | 193 – 200 GPa | 28000 – 29000 ksi | |
Coefficient Poisson’s | 0.29 | 0.29 | |
Impact force Charpy | 325 J | 240 ft-lb | |
Power cut | 86 GPa | 12500 ksi | |
Calculate electric | |||
Resistivity | 7.2e-005 ohm-cm | 7.2e-005 ohm-cm | at 20°C (68°F); 1.16E-04 at 650°C (1200°F) |
Magnetic contagion | 1.008 | 1.008 | at RT |
Heat characteristic | |||
CTE, linear at 20°C | 17.3 µm/m-°C | 9.61 µin/in-°F | from 0-100°C |
CTE, linear at 250°C | 17.8 µm/m-°C | 9.89 µin/in-°F | at 0-315°C (32-600°F) |
CTE, linear at 500°C | 18.7 µm/m-°C | 10.4 µin/in-°F | at 0-650°C |
Heat capacity | 0.5 J/g-°C | 0.12 BTU/lb-°F | from 0-100°C (32-212°F) |
Heat conduction | 16.2 W/m-K | 112 BTU-in/hr-ft²-°F | at 0-100°C, 21.5 W/m°C at 500°C |
Melting temperature | 1400 – 1455 °C | 2550 – 2650 °F | |
Solidus | 1400 °C | 2550 °F | |
Liquidus | 1455 °C | 2650 °F |
Stainless steel angle bar grade SUS316
Equivalent steel grades: UNS S31600, AISI 316, DIN 1.4401, DIN 1.4408, DIN X5CrNiMo17122, TGL 39672 X5CrNiMo1911, TGL 7143X5CrNiMo1811, ISO 2604-1 F62, ISO 2604-2 TS60, ISO 2604-2 TS61, ISO 2604-4 P60 , ISO 2604-4 P61, ISO 4954 X5CrNiMo17122E, ISO 683/13 20, ISO 683/13 20a, ISO 6931 X5CrNiMo17122.
Steel specifications:
Component | Wt. % |
C | 0.08 |
Cr | 17 |
Fe | 65 |
Mn | 2 |
Mo | 2.5 |
Ni | 12 |
P | 0.045 |
S | 0.03 |
Si | 1 |
Physical properties | Metric system | pounds | Annotation |
Proportion | 8 g/cc | 0.289 lb/in³ | |
Mechanical properties | |||
Stiffness Brinell | 149 | 149 | |
Stiffness Knoop | 169 | 169 | Estimated value based on hardness Brinell |
Stiffness Rockwell B | 80 | 80 | |
Stiffness Vickers | 155 | 155 | Estimated value based on hardness Brinell |
Tensile stress | 550 MPa | 79800 psi | |
Flow yield | 240 MPa | 34800 psi | |
Elongation | 60 % | 60 % | in 50 mm |
Elastic module | 193 GPa | 28000 ksi | |
Impact force Charpy | 105 J | 77.4 ft-lb | V-notch |
Izod impact force | 129 J | 95.1 ft-lb | |
Electrical characteristics | |||
Resistivity | 7.4e-005 ohm-cm | 7.4e-005 ohm-cm | at 20ºC |
Magneticity | 1.008 | 1.008 | at RT |
Heat characteristic | |||
CTE, linear at 20°C | 16 µm/m-°C | 8.89 µin/in-°F | 0 – 100ºC |
CTE, linear at 250°C | 16.2 µm/m-°C | 9 µin/in-°F | at 0-315°C (32-600°F) |
CTE, tuyến tính ở 500°C | 17.5 µm/m-°C | 9.72 µin/in-°F | 0 – 540ºC |
Heat capacity | 0.5 J/g-°C | 0.12 BTU/lb-°F | from 0-100°C (32-212°F) |
Heat conduction | 16.3 W/m-K | 113 BTU-in/hr-ft²-°F | 100ºC |
Melting temperature | 1370 – 1400 °C | 2500 – 2550 °F | |
Solidus | 1370 °C | 2500 °F | |
Liquidus | 1400 °C | 2550 °F |